Reduced Shank Drill D120, HSS, BLU

£71.50£95.30

Reduced Shank Drill D120, HSS, BLU

Description

Sutton Tools Reduced Shank Drills are designed to increase the drilling capacity of drill chucks and for slow speed (350 RPM or less), large scale boring. Reduced shanks suit 10mm drill chucks.
Range
Features
Application
Specification
pitem RRP
(inc GST)
Image Info
D1201429 £72
  • D1201429
  • Pack Qty: 1
  • Barcode: 9311963001371
  • Order Multiple: 1
D1201588 £78
  • D1201588
  • Pack Qty: 1
  • Barcode: 9311963000565
  • Order Multiple: 1
D1201905 £95
  • D1201905
  • Pack Qty: 1
  • Barcode: 9311963002439
  • Order Multiple: 1
  • Common Length 6" (152mm) overall length with a 3-3/8" (86mm) flute length
  • Reduced shanks suit 10mm drill chucks
  • 118° standard point for general
  • purpose applications
  • Made from M2 High Speed Steel (HSS) offering the best combination of strength, heat & wear resistance
  • Blue flute with precision ground bright cutting edges making it a better choice when drilling ferrous materials
ISO VDI Description Condition Hardness Strength Optimal
P 1 Steel - Non-alloy, cast & free cutting (~ 0.15 %C) Annealed 125 440
P 2 Steel - Non-alloy, cast & free cutting (~ 0.45 %C) Annealed 190 640
P 3 Steel - Non-alloy, cast & free cutting (~ 0.45 %C) Quenched & Tempered 250 840
P 4 Steel - Non-alloy, cast & free cutting (~ 0.75 %C) Annealed 270 910
P 5 Steel - Non-alloy, cast & free cutting (~ 0.75 %C) Quenched & Tempered 300 1010
P 6 Steel - Low alloy & cast < 5% of alloying elements Annealed 180 610
P 7 Steel - Low alloy & cast < 5% of alloying elements Quenched & Tempered 275 930
P 8 Steel - Low alloy & cast < 5% of alloying elements Quenched & Tempered 300 1010
P 10 Steel - High alloy, cast & tool Annealed 200 680
M 14.1 Stainless Steel - Austenitic Age Hardened 180 610
M 14.2 Stainless Steel - Duplex 250 840
K 15 Cast Iron, Grey (GG) - Ferritic / Pearlitic 180 610
K 17 Cast Iron, Nodular (GGG) - Ferritic 160 570
K 19 Cast Iron, Malleable - Ferritic 130 460
N 21 Aluminum & Magnesium, wrought alloy - Non Heat Treatable 60 210
N 22 Aluminum & Magnesium, wrought alloy - Heat Treatable Age Hardened 100 360
N 23 Aluminum & Magnesium, cast alloy ?12% Si - Non Heat Treatable 75 270
N 24 Aluminum & Magnesium, cast alloy ?12% Si - Heat Treatable Age Hardened 90 320
N 26 Copper & Copper alloys (Brass/Bronze) - Free cutting, Pb > 1% 110 390
N 27 Copper & Copper alloys (Brass/Bronze) - Brass (CuZn, CuSnZn) 90 320
N 28 Copper & Copper alloys (Brass/Bronze) - Bronze (CuSn) 100 360
H 40 Cast Iron - Chilled Cast 400 1350

KEY

Optimal Effective PSteel MStainless KCast Iron NNon-Ferous Metals STitanium & Super Alloys HHard Materials
Designation
N
Material
HSS
Finish
Blu
Max Cut Depth
5XD
Shank Form
A
Helix Angle
R30
Point Tolerance
H8
Point Angle
118°
Point Form
Form A
Cutting Edges
ul