pitem | d1 | tpi | limit | lengthl1mm | lengthl2mm | diameterd2mm | sq | lengthl4mm | z | RRP (inc GST) |
Image | Info |
---|---|---|---|---|---|---|---|---|---|---|---|---|
T4740794 | 5/16 | 26 | Z4 | 72 | 22 | 8 | 6.3 | 9 | 4 | £14 |
|
|
T4740953 | 3/8 | 26 | Z4 | 80 | 24 | 10 | 8 | 11 | 4 | £17 |
|
|
T4741111 | 7/16 | 26 | Z4 | 85 | 25 | 8 | 6.3 | 9 | 4 | £24 |
|
|
T4741270 | 1/2 | 26 | Z4 | 89 | 29 | 9 | 7.1 | 10 | 4 | £22 |
|
|
T4741429 | 9/16 | 26 | Z4 | 95 | 30 | 11.2 | 9 | 12 | 4 | £37 |
|
|
T4741588 | 5/8 | 26 | Z4 | 102 | 32 | 12.5 | 10 | 13 | 4 | £33 |
|
|
T4741905 | 3/4 | 26 | Z4 | 112 | 37 | 14 | 11.2 | 14 | 4 | £48 |
|
|
T4742223 | 7/8 | 26 | Z4 | 118 | 38 | 16 | 12.5 | 16 | 4 | £72 |
|
|
T4742540 | 1 | 26 | Z4 | 130 | 45 | 18 | 14 | 18 | 4 | £83 |
|
ISO | VDI | Description | Condition | Hardness | Strength | Optimal |
---|---|---|---|---|---|---|
P | 1 | Steel - Non-alloy, cast & free cutting (~ 0.15 %C) | Annealed | 125 | 440 | |
P | 2 | Steel - Non-alloy, cast & free cutting (~ 0.45 %C) | Annealed | 190 | 640 | |
P | 3 | Steel - Non-alloy, cast & free cutting (~ 0.45 %C) | Quenched & Tempered | 250 | 840 | |
P | 4 | Steel - Non-alloy, cast & free cutting (~ 0.75 %C) | Annealed | 270 | 910 | |
P | 6 | Steel - Low alloy & cast < 5% of alloying elements | Annealed | 180 | 610 | |
P | 7 | Steel - Low alloy & cast < 5% of alloying elements | Quenched & Tempered | 275 | 930 | |
K | 15 | Cast Iron, Grey (GG) - Ferritic / Pearlitic | 180 | 610 | ||
K | 17 | Cast Iron, Nodular (GGG) - Ferritic | 160 | 570 | ||
K | 19 | Cast Iron, Malleable - Ferritic | 130 | 460 | ||
N | 21 | Aluminum & Magnesium, wrought alloy - Non Heat Treatable | 60 | 210 | ||
N | 22 | Aluminum & Magnesium, wrought alloy - Heat Treatable | Age Hardened | 100 | 360 | |
N | 23 | Aluminum & Magnesium, cast alloy ?12% Si - Non Heat Treatable | 75 | 270 | ||
N | 24 | Aluminum & Magnesium, cast alloy ?12% Si - Heat Treatable | Age Hardened | 90 | 320 | |
N | 26 | Copper & Copper alloys (Brass/Bronze) - Free cutting, Pb > 1% | 110 | 390 | ||
N | 28 | Copper & Copper alloys (Brass/Bronze) - Bronze (CuSn) | 100 | 360 |