ISO TAP T400 Forming, metric, single coolant groove , N, TiN
£26.71 – £30.23
ISO TAP T400 Forming, metric, single coolant groove , N, TiN
£26.71 – £30.23
ISO TAP T400 Forming, metric, single coolant groove , N, TiN
pitem | d1 | limit | lengthl1mm | lengthl2mm | lengthl3mm | diameterd2mm | sq | lengthl4mm | Pitch | RRP (inc GST) |
Image | Info |
---|---|---|---|---|---|---|---|---|---|---|---|---|
T4000300 | M3 | GH4 / 6H | 48 | 11 | 15 | 3.15 | 2.5 | 5 | 0.50 | £30 |
|
|
T4000400 | M4 | GH4 / 6H | 53 | 13 | 18 | 4 | 3.15 | 6 | 0.70 | £27 |
|
|
T4000500 | M5 | GH4 / 6H | 58 | 16 | 22 | 5 | 4 | 7 | 0.80 | £30 |
|
|
T4000600 | M6 | GH4 / 6H | 66 | 19 | 26 | 6.3 | 5 | 8 | 1.00 | £29 |
|
ISO | VDI | Description | Condition | Hardness | Strength | Optimal |
---|---|---|---|---|---|---|
P | 1 | Steel - Non-alloy, cast & free cutting (~ 0.15 %C) | Annealed | 125 | 440 | |
P | 2 | Steel - Non-alloy, cast & free cutting (~ 0.45 %C) | Annealed | 190 | 640 | |
P | 3 | Steel - Non-alloy, cast & free cutting (~ 0.45 %C) | Quenched & Tempered | 250 | 840 | |
P | 4 | Steel - Non-alloy, cast & free cutting (~ 0.75 %C) | Annealed | 270 | 910 | |
P | 6 | Steel - Low alloy & cast < 5% of alloying elements | Annealed | 180 | 610 | |
P | 7 | Steel - Low alloy & cast < 5% of alloying elements | Quenched & Tempered | 275 | 930 | |
M | 14.1 | Stainless Steel - Austenitic | Age Hardened | 180 | 610 | |
N | 21 | Aluminum & Magnesium, wrought alloy - Non Heat Treatable | 60 | 210 | ||
N | 22 | Aluminum & Magnesium, wrought alloy - Heat Treatable | Age Hardened | 100 | 360 | |
N | 23 | Aluminum & Magnesium, cast alloy ?12% Si - Non Heat Treatable | 75 | 270 | ||
N | 24 | Aluminum & Magnesium, cast alloy ?12% Si - Heat Treatable | Age Hardened | 90 | 320 | |
N | 26 | Copper & Copper alloys (Brass/Bronze) - Free cutting, Pb > 1% | 110 | 390 | ||
N | 28 | Copper & Copper alloys (Brass/Bronze) - Bronze (CuSn) | 100 | 360 |