pitem | diameterd1mm | diameterd1inch | lengthl1mm | lengthl2mm | lengthl3mm | diameterd2mm | z | RRP (inc GST) |
Image | Info |
---|---|---|---|---|---|---|---|---|---|---|
E6350300 | 3.00 | NA | 57 | 8 | 19 | 6 | 4 | £20 |
|
|
E6350400 | 4.00 | NA | 57 | 11 | 19 | 6 | 4 | £20 |
|
|
E6350500 | 5.00 | NA | 57 | 13 | 20 | 6 | 4 | £20 |
|
|
E6350600 | 6.00 | NA | 57 | 13 | 21 | 6 | 4 | £16 |
|
|
E6350800 | 8.00 | NA | 63 | 19 | 27 | 8 | 4 | £23 |
|
|
E6351000 | 10.00 | NA | 72 | 22 | 32 | 10 | 4 | £33 |
|
|
E6351200 | 12.00 | NA | 83 | 26 | 38 | 12 | 4 | £43 |
|
|
E6351600 | 16.00 | NA | 92 | 32 | 44 | 16 | 4 | £74 |
|
|
E6352000 | 20.00 | NA | 104 | 38 | 54 | 20 | 4 | £113 |
|
ISO | VDI | Description | Condition | Hardness | Strength | Optimal |
---|---|---|---|---|---|---|
S | 37.3 | Titanium & Titanium alloys - Alpha / Beta alloys | Age Hardened | 1170 | ||
K | 20 | Cast Iron, Malleable - Pearlitic | 230 | 780 | ||
S | 33 | High temperature alloys - Ni / Co based | Annealed | 250 | 840 | |
K | 17 | Cast Iron, Nodular (GGG) - Ferritic | 160 | 570 | ||
N | 21 | Aluminum & Magnesium, wrought alloy - Non Heat Treatable | 60 | 210 | ||
H | 41 | Cast Iron | Hardened & Tempered | 55 | ||
H | 40 | Cast Iron - Chilled | Cast | 400 | 1350 | |
S | 37.1 | Titanium & Titanium alloys - Alpha alloys | 860 | |||
P | 13 | Steel - Corrosion resistant & cast - Martensitic | Quenched & Tempered | 240 | 810 | |
P | 4 | Steel - Non-alloy, cast & free cutting (~ 0.75 %C) | Annealed | 270 | 910 | |
P | 7 | Steel - Low alloy & cast < 5% of alloying elements | Quenched & Tempered | 275 | 930 | |
H | 38.1 | Hardened steel | Hardened & Tempered | 45 | ||
S | 37.4 | Titanium & Titanium alloys - Beta alloys | Annealed | 830 | ||
K | 18 | Cast Iron, Nodular (GGG) - Pearlitic | 250 | 840 | ||
S | 35 | High temperature alloys - Ni / Co based | Cast | 320 | 1080 | |
N | 22 | Aluminum & Magnesium, wrought alloy - Heat Treatable | Age Hardened | 100 | 360 | |
S | 31 | High temperature alloys - Fe based | Annealed | 200 | 680 | |
K | 19 | Cast Iron, Malleable - Ferritic | 130 | 460 | ||
P | 1 | Steel - Non-alloy, cast & free cutting (~ 0.15 %C) | Annealed | 125 | 440 | |
N | 24 | Aluminum & Magnesium, cast alloy ?12% Si - Heat Treatable | Age Hardened | 90 | 320 | |
N | 23 | Aluminum & Magnesium, cast alloy ?12% Si - Non Heat Treatable | 75 | 270 | ||
P | 10 | Steel - High alloy, cast & tool | Annealed | 200 | 680 | |
K | 16 | Cast Iron, Grey (GG) - Pearlitic | 260 | 880 | ||
P | 5 | Steel - Non-alloy, cast & free cutting (~ 0.75 %C) | Quenched & Tempered | 300 | 1010 | |
P | 6 | Steel - Low alloy & cast < 5% of alloying elements | Annealed | 180 | 610 | |
P | 12 | Steel - Corrosion resistant & cast - Ferritic / Martensitic | Annealed | 200 | 680 | |
S | 32 | High temperature alloys - Fe based | Age Hardened | 280 | 950 | |
P | 8 | Steel - Low alloy & cast < 5% of alloying elements | Quenched & Tempered | 300 | 1010 | |
S | 36 | Titanium & Titanium alloys - CP Titanium | 400 | |||
N | 27 | Copper & Copper alloys (Brass/Bronze) - Brass (CuZn, CuSnZn) | 90 | 320 | ||
N | 25 | Aluminum & Magnesium, cast alloy >12% Si - Non Heat Treatable | 130 | 460 | ||
K | 15 | Cast Iron, Grey (GG) - Ferritic / Pearlitic | 180 | 610 | ||
P | 2 | Steel - Non-alloy, cast & free cutting (~ 0.45 %C) | Annealed | 190 | 640 | |
S | 37.2 | Titanium & Titanium alloys - Alpha / Beta alloys | Annealed | 960 | ||
P | 11 | Steel - High alloy, cast & tool | Hardened & Tempered | 325 | 1100 | |
P | 9 | Steel - Low alloy & cast < 5% of alloying elements | Quenched & Tempered | 350 | 1180 | |
P | 3 | Steel - Non-alloy, cast & free cutting (~ 0.45 %C) | Quenched & Tempered | 250 | 840 |