DIN TAP T141 Gun, Metric, NH, M, TiAIN

£44.83£112.65

DIN TAP T141 Gun, Metric, NH, M, TiAIN

Description

DIN TAP T141 Gun, Metric, NH, M, TiAIN.  Suitable for harder materials up to 42 HRC.  Through holes. Depths up to 3 x d1
Range
Features
Application
Specification
pitemd1Pitchlimitlengthl1mmlengthl2mmdiameterd2mmsqlengthl4mmz RRP
(inc GST)
Image Info
T1411200 M12 1.75 ISO 2 / 6H 110 28 9 7 10 3 £45
  • T1411200
  • M12
  • ISO 2 / 6H
  • 110
  • 28
  • 9
  • 7
  • 10
  • 3
  • Pack Qty: 1
  • Barcode: 9311963413211
  • Order Multiple: 1
T1411400 M14 2 ISO 2 / 6H 110 30 11 9 12 3 £58
  • T1411400
  • M14
  • ISO 2 / 6H
  • 110
  • 30
  • 11
  • 9
  • 12
  • 3
  • Pack Qty: 1
  • Barcode: 9311963413228
  • Order Multiple: 1
T1411600 M16 2 ISO 2 / 6H 110 32 12 9 12 4 £65
  • T1411600
  • M16
  • ISO 2 / 6H
  • 110
  • 32
  • 12
  • 9
  • 12
  • 4
  • Pack Qty: 1
  • Barcode: 9311963413235
  • Order Multiple: 1
T1411800 M18 2.5 ISO 2 / 6H 125 34 14 11 14 4 £87
  • T1411800
  • M18
  • ISO 2 / 6H
  • 125
  • 34
  • 14
  • 11
  • 14
  • 4
  • Pack Qty: 1
  • Barcode: 9311963413242
  • Order Multiple: 1
T1412000 M20 2.5 ISO 2 / 6H 140 34 16 12 15 4 £113
  • T1412000
  • M20
  • ISO 2 / 6H
  • 140
  • 34
  • 16
  • 12
  • 15
  • 4
  • Pack Qty: 1
  • Barcode: 9311963413259
  • Order Multiple: 1
  • Suitable for harder short chipping materials up to 42 HRc
  • Through holes
  • Depths up to 3 x d1
ISO VDI Description Condition Hardness Strength Optimal
P 3 Steel - Non-alloy, cast & free cutting (~ 0.45 %C) Quenched & Tempered 250 840
P 4 Steel - Non-alloy, cast & free cutting (~ 0.75 %C) Annealed 270 910
P 5 Steel - Non-alloy, cast & free cutting (~ 0.75 %C) Quenched & Tempered 300 1010
P 7 Steel - Low alloy & cast < 5% of alloying elements Quenched & Tempered 275 930
P 8 Steel - Low alloy & cast < 5% of alloying elements Quenched & Tempered 300 1010
P 9 Steel - Low alloy & cast < 5% of alloying elements Quenched & Tempered 350 1180
P 10 Steel - High alloy, cast & tool Annealed 200 680
P 11 Steel - High alloy, cast & tool Hardened & Tempered 325 1100
P 12 Steel - Corrosion resistant & cast - Ferritic / Martensitic Annealed 200 680
P 13 Steel - Corrosion resistant & cast - Martensitic Quenched & Tempered 240 810
M 14.1 Stainless Steel - Austenitic Age Hardened 180 610
M 14.2 Stainless Steel - Duplex 250 840
M 14.3 Stainless Steel - Precipitation Hardening 250 840
K 15 Cast Iron, Grey (GG) - Ferritic / Pearlitic 180 610
K 16 Cast Iron, Grey (GG) - Pearlitic 260 880
K 17 Cast Iron, Nodular (GGG) - Ferritic 160 570
K 18 Cast Iron, Nodular (GGG) - Pearlitic 250 840
K 19 Cast Iron, Malleable - Ferritic 130 460
K 20 Cast Iron, Malleable - Pearlitic 230 780
N 23 Aluminum & Magnesium, cast alloy ?12% Si - Non Heat Treatable 75 270
N 24 Aluminum & Magnesium, cast alloy ?12% Si - Heat Treatable Age Hardened 90 320
N 25 Aluminum & Magnesium, cast alloy >12% Si - Non Heat Treatable 130 460
N 26 Copper & Copper alloys (Brass/Bronze) - Free cutting, Pb > 1% 110 390
N 27 Copper & Copper alloys (Brass/Bronze) - Brass (CuZn, CuSnZn) 90 320
N 28 Copper & Copper alloys (Brass/Bronze) - Bronze (CuSn) 100 360
H 38.1 Hardened steel Hardened & Tempered 45
H 40 Cast Iron - Chilled Cast 400 1350

KEY

Optimal Effective PSteel MStainless KCast Iron NNon-Ferous Metals STitanium & Super Alloys HHard Materials
Designation
NH
Material
PM-HSSE V3
Finish
TiAIN
Max Cut Depth
3xD
Shank Form
A
Standard
DIN376
Thread Form
M
Nut Tolerance
ISO 2 / 6H
Lead
Form B / 4.5 x P