ISO | VDI | Description | Condition | Hardness | Strength | Optimal |
---|---|---|---|---|---|---|
P | 1 | Steel - Non-alloy, cast & free cutting (~ 0.15 %C) | Annealed | 125 | 440 | |
P | 2 | Steel - Non-alloy, cast & free cutting (~ 0.45 %C) | Annealed | 190 | 640 | |
P | 3 | Steel - Non-alloy, cast & free cutting (~ 0.45 %C) | Quenched & Tempered | 250 | 840 | |
P | 4 | Steel - Non-alloy, cast & free cutting (~ 0.75 %C) | Annealed | 270 | 910 | |
P | 5 | Steel - Non-alloy, cast & free cutting (~ 0.75 %C) | Quenched & Tempered | 300 | 1010 | |
P | 6 | Steel - Low alloy & cast < 5% of alloying elements | Annealed | 180 | 610 | |
P | 7 | Steel - Low alloy & cast < 5% of alloying elements | Quenched & Tempered | 275 | 930 | |
P | 8 | Steel - Low alloy & cast < 5% of alloying elements | Quenched & Tempered | 300 | 1010 | |
P | 10 | Steel - High alloy, cast & tool | Annealed | 200 | 680 | |
P | 12 | Steel - Corrosion resistant & cast - Ferritic / Martensitic | Annealed | 200 | 680 | |
M | 14.1 | Stainless Steel - Austenitic | Age Hardened | 180 | 610 | |
M | 14.2 | Stainless Steel - Duplex | 250 | 840 | ||
M | 14.3 | Stainless Steel - Precipitation Hardening | 250 | 840 | ||
K | 15 | Cast Iron, Grey (GG) - Ferritic / Pearlitic | 180 | 610 | ||
K | 16 | Cast Iron, Grey (GG) - Pearlitic | 260 | 880 | ||
K | 17 | Cast Iron, Nodular (GGG) - Ferritic | 160 | 570 | ||
K | 18 | Cast Iron, Nodular (GGG) - Pearlitic | 250 | 840 | ||
K | 19 | Cast Iron, Malleable - Ferritic | 130 | 460 | ||
N | 21 | Aluminum & Magnesium, wrought alloy - Non Heat Treatable | 60 | 210 | ||
N | 22 | Aluminum & Magnesium, wrought alloy - Heat Treatable | Age Hardened | 100 | 360 | |
N | 23 | Aluminum & Magnesium, cast alloy ?12% Si - Non Heat Treatable | 75 | 270 | ||
N | 24 | Aluminum & Magnesium, cast alloy ?12% Si - Heat Treatable | Age Hardened | 90 | 320 | |
N | 25 | Aluminum & Magnesium, cast alloy >12% Si - Non Heat Treatable | 130 | 460 | ||
N | 26 | Copper & Copper alloys (Brass/Bronze) - Free cutting, Pb > 1% | 110 | 390 | ||
N | 27 | Copper & Copper alloys (Brass/Bronze) - Brass (CuZn, CuSnZn) | 90 | 320 | ||
N | 28 | Copper & Copper alloys (Brass/Bronze) - Bronze (CuSn) | 100 | 360 | ||
N | 29 | Non-metallic - Thermosetting & fiber-reinforced plastics | ||||
S | 31 | High temperature alloys - Fe based | Annealed | 200 | 680 | |
S | 32 | High temperature alloys - Fe based | Age Hardened | 280 | 950 | |
S | 33 | High temperature alloys - Ni / Co based | Annealed | 250 | 840 | |
S | 36 | Titanium & Titanium alloys - CP Titanium | 400 | |||
S | 37.1 | Titanium & Titanium alloys - Alpha alloys | 860 | |||
S | 37.2 | Titanium & Titanium alloys - Alpha / Beta alloys | Annealed | 960 | ||
S | 37.4 | Titanium & Titanium alloys - Beta alloys | Annealed | 830 | ||
H | 40 | Cast Iron - Chilled | Cast | 400 | 1350 |