pitem | diameterd1mm | diameterd1inch | lengthl1mm | lengthl2mm | diameterd2mm | z | RRP (inc GST) |
Image | Info |
---|---|---|---|---|---|---|---|---|---|
E5470400 | 4.00 | NA | 57 | 11 | 6 | 3 | £50 |
|
|
E5470500 | 5.00 | NA | 57 | 13 | 6 | 3 | £50 |
|
|
E5470600 | 6.00 | NA | 57 | 13 | 6 | 3 | £47 |
|
|
E5470800 | 8.00 | NA | 63 | 19 | 8 | 3 | £54 |
|
|
E5471000 | 10.00 | NA | 72 | 22 | 10 | 4 | £59 |
|
|
E5471200 | 12.00 | NA | 83 | 26 | 12 | 4 | £70 |
|
|
E5471600 | 16.00 | NA | 92 | 32 | 16 | 4 | £111 |
|
|
E5472000 | 20.00 | NA | 104 | 38 | 20 | 4 | £166 |
|
ISO | VDI | Description | Condition | Hardness | Strength | Optimal |
---|---|---|---|---|---|---|
P | 1 | Steel - Non-alloy, cast & free cutting (~ 0.15 %C) | Annealed | 125 | 440 | |
P | 2 | Steel - Non-alloy, cast & free cutting (~ 0.45 %C) | Annealed | 190 | 640 | |
P | 3 | Steel - Non-alloy, cast & free cutting (~ 0.45 %C) | Quenched & Tempered | 250 | 840 | |
P | 4 | Steel - Non-alloy, cast & free cutting (~ 0.75 %C) | Annealed | 270 | 910 | |
P | 5 | Steel - Non-alloy, cast & free cutting (~ 0.75 %C) | Quenched & Tempered | 300 | 1010 | |
P | 6 | Steel - Low alloy & cast < 5% of alloying elements | Annealed | 180 | 610 | |
P | 7 | Steel - Low alloy & cast < 5% of alloying elements | Quenched & Tempered | 275 | 930 | |
P | 8 | Steel - Low alloy & cast < 5% of alloying elements | Quenched & Tempered | 300 | 1010 | |
P | 10 | Steel - High alloy, cast & tool | Annealed | 200 | 680 | |
K | 17 | Cast Iron, Nodular (GGG) - Ferritic | 160 | 570 | ||
N | 21 | Aluminum & Magnesium, wrought alloy - Non Heat Treatable | 60 | 210 | ||
N | 22 | Aluminum & Magnesium, wrought alloy - Heat Treatable | Age Hardened | 100 | 360 | |
N | 23 | Aluminum & Magnesium, cast alloy ?12% Si - Non Heat Treatable | 75 | 270 | ||
N | 24 | Aluminum & Magnesium, cast alloy ?12% Si - Heat Treatable | Age Hardened | 90 | 320 | |
N | 25 | Aluminum & Magnesium, cast alloy >12% Si - Non Heat Treatable | 130 | 460 |