TAP PIPE 3/4 UNI NPT 374 BRT
£25.62 – £104.37
pitem | d1 | tpi | limit | lengthl1mm | lengthl2mm | diameterd2mm | sq | lengthl4mm | z | RRP (inc GST) |
Image | Info |
---|---|---|---|---|---|---|---|---|---|---|---|---|
T3081029 | 1/8 | 27 | ANSI B1.20.1 | 90 | 20 | 7 | 5.5 | 8 | 4 | £26 |
|
|
T3081372 | 1/4 | 18 | ANSI B1.20.1 | 100 | 22 | 11 | 9 | 12 | 4 | £37 |
|
|
T3081716 | 3/8 | 18 | ANSI B1.20.1 | 100 | 22 | 12 | 9 | 12 | 4 | £39 |
|
|
T3082134 | 1/2 | 14 | ANSI B1.20.1 | 125 | 25 | 16 | 12 | 15 | 4 | £50 |
|
|
T3082667 | 3/4 | 14 | ANSI B1.20.1 | 140 | 28 | 20 | 16 | 19 | 4 | £74 |
|
|
T3083340 | 1 | 12 | ANSI B1.20.1 | 160 | 30 | 25 | 20 | 23 | 5 | £104 |
|
ISO | VDI | Description | Condition | Hardness | Strength | Optimal |
---|---|---|---|---|---|---|
P | 1 | Steel - Non-alloy, cast & free cutting (~ 0.15 %C) | Annealed | 125 | 440 | |
P | 2 | Steel - Non-alloy, cast & free cutting (~ 0.45 %C) | Annealed | 190 | 640 | |
P | 3 | Steel - Non-alloy, cast & free cutting (~ 0.45 %C) | Quenched & Tempered | 250 | 840 | |
P | 4 | Steel - Non-alloy, cast & free cutting (~ 0.75 %C) | Annealed | 270 | 910 | |
P | 5 | Steel - Non-alloy, cast & free cutting (~ 0.75 %C) | Quenched & Tempered | 300 | 1010 | |
P | 6 | Steel - Low alloy & cast < 5% of alloying elements | Annealed | 180 | 610 | |
P | 7 | Steel - Low alloy & cast < 5% of alloying elements | Quenched & Tempered | 275 | 930 | |
P | 8 | Steel - Low alloy & cast < 5% of alloying elements | Quenched & Tempered | 300 | 1010 | |
P | 10 | Steel - High alloy, cast & tool | Annealed | 200 | 680 | |
P | 12 | Steel - Corrosion resistant & cast - Ferritic / Martensitic | Annealed | 200 | 680 | |
P | 13 | Steel - Corrosion resistant & cast - Martensitic | Quenched & Tempered | 240 | 810 | |
M | 14.1 | Stainless Steel - Austenitic | Age Hardened | 180 | 610 | |
M | 14.2 | Stainless Steel - Duplex | 250 | 840 | ||
M | 14.3 | Stainless Steel - Precipitation Hardening | 250 | 840 | ||
K | 15 | Cast Iron, Grey (GG) - Ferritic / Pearlitic | 180 | 610 | ||
K | 17 | Cast Iron, Nodular (GGG) - Ferritic | 160 | 570 | ||
K | 19 | Cast Iron, Malleable - Ferritic | 130 | 460 | ||
K | 20 | Cast Iron, Malleable - Pearlitic | 230 | 780 | ||
N | 21 | Aluminum & Magnesium, wrought alloy - Non Heat Treatable | 60 | 210 | ||
N | 22 | Aluminum & Magnesium, wrought alloy - Heat Treatable | Age Hardened | 100 | 360 | |
N | 23 | Aluminum & Magnesium, cast alloy ?12% Si - Non Heat Treatable | 75 | 270 | ||
N | 24 | Aluminum & Magnesium, cast alloy ?12% Si - Heat Treatable | Age Hardened | 90 | 320 | |
N | 26 | Copper & Copper alloys (Brass/Bronze) - Free cutting, Pb > 1% | 110 | 390 | ||
N | 27 | Copper & Copper alloys (Brass/Bronze) - Brass (CuZn, CuSnZn) | 90 | 320 | ||
N | 28 | Copper & Copper alloys (Brass/Bronze) - Bronze (CuSn) | 100 | 360 |