TAP GUN MF12X1 6HX VAPM TiCN
£30.71 – £116.16
pitem | d1 | limit | lengthl1mm | lengthl2mm | diameterd2mm | sq | lengthl4mm | z | RRP (inc GST) |
Image | Info |
---|---|---|---|---|---|---|---|---|---|---|---|
T1600604 | MF6 | 6HX | 80 | 14 | 4.5 | 3.4 | 6 | 3 | £31 |
|
|
T1600803 | MF8 | 6HX | 80 | 18 | 6 | 4.9 | 8 | 3 | £33 |
|
|
T1601004 | MF10 | 6HX | 90 | 20 | 7 | 5.5 | 8 | 3 | £38 |
|
|
T1601005 | MF10 | 6HX | 90 | 20 | 7 | 5.5 | 8 | 3 | £37 |
|
|
T1601205 | MF12 | 6HX | 100 | 22 | 9 | 7 | 10 | 3 | £48 |
|
|
T1601206 | MF12 | 6HX | 100 | 22 | 9 | 7 | 10 | 3 | £45 |
|
|
T1601207 | MF12 | 6HX | 100 | 22 | 9 | 7 | 10 | 3 | £45 |
|
|
T1601405 | MF14 | 6HX | 100 | 22 | 11 | 9 | 12 | 3 | £63 |
|
|
T1601406 | MF14 | 6HX | 100 | 22 | 11 | 9 | 12 | 3 | £60 |
|
|
T1601605 | MF16 | 6HX | 100 | 22 | 12 | 9 | 12 | 3 | £66 |
|
|
T1601807 | MF18 | 6HX | 110 | 25 | 14 | 11 | 14 | 4 | £88 |
|
|
T1602005 | MF20 | 6HX | 125 | 25 | 16 | 12 | 15 | 4 | £116 |
|
ISO | VDI | Description | Condition | Hardness | Strength | Optimal |
---|---|---|---|---|---|---|
P | 1 | Steel - Non-alloy, cast & free cutting (~ 0.15 %C) | Annealed | 125 | 440 | |
P | 2 | Steel - Non-alloy, cast & free cutting (~ 0.45 %C) | Annealed | 190 | 640 | |
P | 3 | Steel - Non-alloy, cast & free cutting (~ 0.45 %C) | Quenched & Tempered | 250 | 840 | |
P | 4 | Steel - Non-alloy, cast & free cutting (~ 0.75 %C) | Annealed | 270 | 910 | |
P | 6 | Steel - Low alloy & cast < 5% of alloying elements | Annealed | 180 | 610 | |
P | 7 | Steel - Low alloy & cast < 5% of alloying elements | Quenched & Tempered | 275 | 930 | |
P | 10 | Steel - High alloy, cast & tool | Annealed | 200 | 680 | |
P | 12 | Steel - Corrosion resistant & cast - Ferritic / Martensitic | Annealed | 200 | 680 | |
P | 13 | Steel - Corrosion resistant & cast - Martensitic | Quenched & Tempered | 240 | 810 | |
M | 14.1 | Stainless Steel - Austenitic | Age Hardened | 180 | 610 | |
M | 14.2 | Stainless Steel - Duplex | 250 | 840 | ||
M | 14.3 | Stainless Steel - Precipitation Hardening | 250 | 840 | ||
N | 21 | Aluminum & Magnesium, wrought alloy - Non Heat Treatable | 60 | 210 | ||
N | 22 | Aluminum & Magnesium, wrought alloy - Heat Treatable | Age Hardened | 100 | 360 | |
N | 23 | Aluminum & Magnesium, cast alloy ?12% Si - Non Heat Treatable | 75 | 270 | ||
N | 24 | Aluminum & Magnesium, cast alloy ?12% Si - Heat Treatable | Age Hardened | 90 | 320 | |
N | 25 | Aluminum & Magnesium, cast alloy >12% Si - Non Heat Treatable | 130 | 460 | ||
N | 26 | Copper & Copper alloys (Brass/Bronze) - Free cutting, Pb > 1% | 110 | 390 | ||
N | 28 | Copper & Copper alloys (Brass/Bronze) - Bronze (CuSn) | 100 | 360 | ||
S | 31 | High temperature alloys - Fe based | Annealed | 200 | 680 | |
S | 32 | High temperature alloys - Fe based | Age Hardened | 280 | 950 | |
S | 33 | High temperature alloys - Ni / Co based | Annealed | 250 | 840 |