Carbide Endmill, E524 R45 W, DIN6527L – 3 Flute
£16.64 – £127.25
Carbide Endmill, E524 R45 W, DIN6527L – 3 Flute
£16.64 – £127.25
Carbide Endmill, E524 R45 W, DIN6527L – 3 Flute
pitem | diameterd1mm | diameterd1inch | lengthl1mm | lengthl2mm | diameterd2mm | z | RRP (inc GST) |
Image | Info |
---|---|---|---|---|---|---|---|---|---|
E5240300 | 3.00 | NA | 57 | 7 | 6 | 3 | £17 |
|
|
E5240400 | 4.00 | NA | 57 | 8 | 6 | 3 | £17 |
|
|
E5240500 | 5.00 | NA | 57 | 10 | 6 | 3 | £17 |
|
|
E5240600 | 6.00 | NA | 57 | 10 | 6 | 3 | £17 |
|
|
E5240800 | 8.00 | NA | 63 | 16 | 8 | 3 | £22 |
|
|
E5241000 | 10.00 | NA | 72 | 19 | 10 | 3 | £31 |
|
|
E5241200 | 12.00 | NA | 83 | 22 | 12 | 3 | £47 |
|
|
E5241600 | 16.00 | NA | 92 | 26 | 16 | 3 | £80 |
|
|
E5242000 | 20.00 | NA | 104 | 32 | 20 | 3 | £127 |
|
ISO | VDI | Description | Condition | Hardness | Strength | Optimal |
---|---|---|---|---|---|---|
N | 21 | Aluminum & Magnesium, wrought alloy - Non Heat Treatable | 60 | 210 | ||
N | 22 | Aluminum & Magnesium, wrought alloy - Heat Treatable | Age Hardened | 100 | 360 | |
N | 23 | Aluminum & Magnesium, cast alloy ?12% Si - Non Heat Treatable | 75 | 270 | ||
N | 24 | Aluminum & Magnesium, cast alloy ?12% Si - Heat Treatable | Age Hardened | 90 | 320 | |
N | 25 | Aluminum & Magnesium, cast alloy >12% Si - Non Heat Treatable | 130 | 460 | ||
N | 26 | Copper & Copper alloys (Brass/Bronze) - Free cutting, Pb > 1% | 110 | 390 | ||
N | 27 | Copper & Copper alloys (Brass/Bronze) - Brass (CuZn, CuSnZn) | 90 | 320 | ||
N | 28 | Copper & Copper alloys (Brass/Bronze) - Bronze (CuSn) | 100 | 360 |